For most small driveway cracks, use a pourable or tube crack filler—it’s thicker, stays in the crack, and works on gaps up to about 1/2 inch wide. Choose a liquid crack sealer when you need to coat a wide, shallow area or want to seal the whole surface against moisture, because it’s thinner and spreads out. The real difference comes down to crack size and whether you’re patching a gap or coating the pavement.

Worked Example: Sealing a 1/4-Inch Crack in Asphalt

Here’s the same task—fixing a 1/4-inch wide, 3-foot long crack in an asphalt driveway—done with each product, so you can see how they behave.

Using a Crack Filler (Pourable or Tube)

Clean the crack with a wire brush and blow out dust with a leaf blower or shop vac. If the crack is deeper than 1 inch, stuff backer rod foam into it so the filler doesn’t sink. Pour or squeeze the filler into the crack, slightly overfilling it, then use a putty knife to strike it flush with the driveway surface. Let it cure for 24 hours before driving on it. The filler stays flexible and won’t run out, even on a hot day.

Using a Liquid Crack Sealer (Self-Leveling)

Clean the crack the same way. Pour the liquid sealer directly from the jug, starting at one end and moving slowly so it flows into the gap. Because it’s thin, it will level itself and may sink into deep cracks, so you might need a second coat after the first dries (usually 2–4 hours). It’s great for hairline cracks (under 1/8 inch) where a thick filler won’t penetrate. For a 1/4-inch crack, you’ll likely need two passes, and the sealer may leave a slight film on the surface around the crack.

For this size crack, the filler wins because it fills the gap in one pass and doesn’t waste product. The sealer works, but it’s better suited to tiny, shallow cracks.

Crack Sealer vs Filler: Side-by-Side Comparison

Attribute Crack Filler Crack Sealer
Consistency Thick, paste-like or pourable with sand Thin, liquid, self-leveling
Best for crack width 1/8 to 1/2 inch (3–12 mm) Hairline to 1/8 inch (under 3 mm)
Fills deep gaps Yes, stays in place No, may sink; needs multiple coats
Surface coating No, stays in the crack Yes, can seal a wide area
Cure time before driving 24 hours typically 4–6 hours for light traffic, 24 hours for full cure
Tools needed Putty knife, caulk gun (if tube) Pour spout or brush
Best surface Asphalt and concrete Asphalt mainly, some for concrete

Which One Should You Use? The General Rule

Measure the crack width with a coin or tape measure. If it’s wider than 1/8 inch (about the thickness of a dime), use a crack filler. If it’s a hairline crack or a network of tiny cracks, use a liquid sealer. For cracks wider than 1/2 inch, you need a patching compound, not a filler or sealer.

Also consider the surface. On asphalt, both work, but fillers often contain asphalt emulsion that blends better. On concrete, use a concrete-specific filler or sealer, because asphalt-based products can stain. If the crack is actively growing or water pools in it, fix the drainage issue first—sealing a crack that keeps widening won’t last.

Cost and Upkeep: Filler vs Sealer Over Time

Crack filler costs more per ounce than sealer, but you use less of it because it stays in the crack. A 1-gallon jug of filler covers about 100–150 linear feet of 1/4-inch crack, while a 1-gallon jug of sealer covers about 200–300 square feet of surface when used as a coating. For a single crack, filler is cheaper. For a whole driveway with many hairline cracks, sealer is more economical.

Upkeep differs too. Filler lasts 2–3 years in most climates, but it can crack or pull out if the driveway shifts. Sealer forms a thin film that wears away in 1–2 years, especially in high-traffic areas or harsh sun. Reapplying sealer is easy—just clean and pour. Reapplying filler requires digging out old material if it failed. In cold climates, both need to be applied when the temperature is above 50°F (10°C) and the surface is dry, or they won’t bond.

How to Prep the Crack for Either Product

Good prep makes both products last longer. Start by removing loose debris with a wire brush or stiff broom. For deep cracks, use a shop vac to pull out dirt and dust. If the crack is damp, wait for a dry day—moisture prevents adhesion. For oily stains near the crack, scrub with a degreaser and rinse, then let dry completely.

If the crack is wider than 1/2 inch, fill it with sand or backer rod before applying filler. For sealer, you can brush it into the crack with a small paintbrush to work it in. Always read the label for specific prep steps, as some products require priming the crack with water or a bonding agent.

Can You Use Filler as a Sealer or Vice Versa?

You can use a filler on a hairline crack, but it’s messy—the thick paste won’t flow into the gap, so you’ll leave excess on the surface that can peel. You can use a sealer on a wide crack, but it will sink and leave a depression that collects water. For best results, match the product to the crack size. If you have a mix of crack sizes, use filler for the wide ones and sealer for the hairline ones. Some products are labeled “filler/sealer”—these are usually a middle-ground consistency that works on cracks up to 1/4 inch, but they don’t excel at either extreme.

What About Crack Widths Over 1/2 Inch?

If your crack is wider than 1/2 inch, neither filler nor sealer is the right tool. Use a driveway patching compound, which comes as a mix you trowel into the gap. For very large areas, you may need to replace the section of driveway. Patching compound is thicker and contains aggregate, so it can bridge gaps without sinking. Apply it in layers if the crack is deep, letting each layer cure. This is a different product, so don’t substitute filler or sealer for it.

When to Call a Professional for Driveway Cracks

If the crack is accompanied by a sunken or raised edge (more than 1/4 inch difference), or if the crack runs the full length of the driveway and is getting wider, the problem may be a failing base, not just the surface. In that case, sealing or filling won’t fix it—you need a contractor to assess the subgrade. Also, if you see vegetation growing through the crack or water seeping up, there may be drainage issues that need professional attention. For simple surface cracks, DIY is fine, but for structural issues, call a paving contractor.